  I used an oil-varnish blend
  Posted by: bnystrom on Nov-02-12 7:11 AM (EST)
 

It's the same 50:50 blend of tung oil and varnish that I use on all of my paddles. The finish does wear off, but it's quick and easy to renew. The underlying oak is hard enough that it never wore appreciably.